[1] Yanyun, Bai, Kewei Gao, Xiaolu Pang*, et. al., Brittle coating effects on fatigue cracks behavior in Ti alloys, International Journal of Fatigue 125(2019), pp.432-439
[2] Tao Guo, Xiaolu Pang*, et. al., Substrate slip steps promote cracking and buckling of thin brittle film, Scripta Materialia, 163(2019), pp.82-85
[3] Rongjian Shi, Lijie Qiao, Xiaolu Pang*, et. al., Microstructure evolution of in-situ nanoparticles and its comprehensive effect on high strength steel, Journal of Materials Science & Technology, 35 (2019), pp.1940-1950
[4] Shanshan Zhang, Huisheng Yang, Kewei Gao, Xiaolu Pang*, et. al., Comparative study of Ti and Cr adhesion to the AlN ceramic: Experiments and calculations, Applied Surface Science, 457(2018), pp.856-862
[5] Tao Guo, Yanmeng Chen, Xiaolu Pang*, et. al., Cleavage cracking of ductile-metal substrates induced by brittle coating fracture, Acta Materialia, 152(2018), pp.77-85
[6] Tao Guo, Xiaolu Pang*, et. al., High temperature brittle film adhesion measured from annealing-induced circular blisters, Acta Materialia, 139(2017), pp.1-9
[7] Tao Guo, Lijie Qiao, Xiaolu Pang*, et. al., Brittle film-induced cracking of ductile substrates, Acta materialia, 99(2016), pp.273-280